Tape Unwinding and Tension Control on a Draw Tape Garbage Bag Making Machine
November 19, 2026

Tape Unwinding and Tension Control on a Draw Tape Garbage Bag Making Machine

A draw tape garbage bag fails in the customer’s hand, not on the machine. The tape pulls out of the hem, the drawstring snaps, or one side will not cinch. By then the roll has shipped, and the cause is usually two weeks and forty metres of film behind: an unwind tension that was set once and never revisited.

Tape feeding is the part of a draw tape garbage bag making machine that gets the least attention and causes the most complaints. This article covers how the tape path works, where tension is lost, and how to set it so the drawstring behaves the same on the first bag of the roll and the last.

What the Tape Path Actually Has to Do

A draw tape bag is a tube of film with a folded hem at the top, and a tape threaded inside that hem before the hem is sealed. Four things have to be true at once:

● The tape must arrive at the hem at the same speed as the film — any speed difference shows up as slack tape (which bunches) or tight tape (which puckers the hem).

● The tape must sit at a consistent depth — too shallow and the hem seal misses it, too deep and the tape cannot be gripped when the user pulls.

● The tape must not twist — a half-twist becomes a flat spot that will not slide in the hem, and the bag tears when the user pulls hard.

● The tension must not change as the tape roll runs down — a roll that starts at 300 mm diameter and ends at 80 mm presents a very different inertia and brake requirement.

The CW-1000PG+OR draw tape machine runs at up to 60 m/min with 500 to 1,100 mm bag widths, which is fast enough that tension errors become visible within a few metres rather than a few hundred bags.

Three Tension Zones, Three Different Problems

Operators often talk about “tension” as one setting. It is three, and they interact:

● Main film unwind — sets the baseline web tension. Too high and the film stretches, so bag length drifts as the roll runs down; too low and the web wanders, producing wrinkles at the hem fold.

● Tape unwind — sets how the tape enters the hem. This is the zone that decides whether the drawstring works, and it deserves its own control rather than a friction pad.

● Post-hem take-up — after the hem is sealed, the combined web has different stiffness. If take-up tension is set for film alone, the hem edge cockles.

A machine with independent servo control on film and tape handles this with two setpoints. A machine with a single brake handles it by compromise, which is why tape defects cluster at the extremes of roll diameter.

Dancer, Load Cell or Torque Mode

Three common ways to hold tape tension, each with a distinct behaviour:

● Dancer arm — a spring-loaded or pneumatic roller that absorbs speed differences. Simple, robust, and it buffers short transients well. Its weakness is inertia: a heavy dancer responds slowly at high speed, and a light one oscillates.

● Load cell with closed-loop control — measures actual web tension and corrects the drive. The most accurate option, and the one that keeps tension constant as the roll diameter changes. It needs calibration and a clean signal.

● Torque mode on a servo or clutch — the drive applies a calculated torque that decreases as roll diameter falls. Cheap and effective if the diameter is tracked accurately; if the diameter estimate is wrong, tension drifts silently.

Most Chinese draw tape machines use a dancer for the film and either torque mode or a small dancer for the tape. When a customer reports inconsistent drawstring performance, the first question is which of these the tape uses, because the fixes differ completely.

CW-1000PG+OR draw tape garbage bag machine overlap roll

Setting Tape Tension: A Method, Not a Number

There is no universal tension value, because tape width, tape thickness and machine speed all change the answer. Use a method instead:

● Start slack and increase — begin with the tape visibly loose, then increase in small steps until the hem lies flat with no puckering. Tension that is too high puckers first, then tears the hem seal.

● Test at three roll diameters — full, half and near-empty tape roll. If the hem looks different at each, the control is not compensating and the dancer or diameter tracking needs attention.

● Test at two speeds — 50 percent and full production speed. Tension that holds at low speed and sags at high speed points to a response problem, not a setpoint problem.

● Pull test the finished bag — grip the tape and pull firmly. The tape should slide in the hem without tearing the film, and the hem seal should not open. If the tape snaps, it was over-tensioned during sealing; if it pulls out, the hem seal did not capture it.

Write the accepted settings on the machine card for that product. Tape tension is one of the parameters most often lost between shifts.

Five Tape Defects and Their Real Causes

Each symptom has a short list of likely causes, in order of frequency:

● Hem puckering — tape tension too high, or tape entering faster than the film. Check the tape drive ratio before adjusting the dancer.

● Slack tape inside the hem — tape tension too low, or a tape roll that is wound loosely at the supplier. Squeeze the roll: if it deflects easily, the problem arrived with the material.

● Tape twist — the tape path has a roller that is not parallel, or the tape is being pulled from the side of the roll rather than the centre. A twist of half a turn is enough to jam the hem.

● Tape not captured by the hem seal — tape sitting too deep, sealing temperature low, or the hem fold not fully closed before sealing. Check fold first: a hem that is not flat cannot be sealed around a tape.

● Tape breaks during use — over-tension at sealing, sharp edge at the hem fold, or a tape grade too weak for the bag size. A 500 mm bag and a 1,100 mm bag should not use the same tape thickness.

There is a sixth that is not a tape defect at all: a bag that tears below the hem when pulled. That is a film or seal issue, and adjusting tape tension makes it worse.

Splicing Tape Without Stopping the Line

Tape rolls end, and how the splice is made decides whether the next hundred bags are good:

● Overlap splice, not butt splice — a butt splice has no strength and will part in the hem. Overlap by 20 to 30 mm and secure it flat.

● Keep the splice flat — a lump in the tape becomes a bump in the hem, and a bump becomes a leak or a tear. Press the splice and check with a finger before restarting.

● Mark the splice position — the bags containing the splice should be removed at winding. A chalk mark or a counter offset does this without stopping production.

● Prepare the next roll in advance — tape rolls are light and can be staged on a shelf above the machine, so the change takes seconds rather than minutes.

CW-1000PG+OR draw tape garbage bag machine tape path

Maintenance That Keeps Tension Predictable

Most tension problems are mechanical before they are electrical:

● Roller bearings — a dry bearing in the tape path adds drag that varies with load. Spin every roller by hand weekly; a roller that does not coast is a roller that is stealing tension.

● Dancer pivot — must move freely with no play. Clean and lubricate monthly; a sticky pivot produces tension that steps rather than varies smoothly.

● Brake or clutch pads — wear changes the torque curve. Inspect quarterly and replace as a set.

● Load cell calibration — if the machine uses one, re-zero monthly and verify with a known weight. A drifting zero produces a machine that behaves differently every morning.

● Guide alignment — a roller out of parallel by a millimetre over a 500 mm span will pull the tape sideways over a shift. Check with a straight edge after any maintenance that disturbs the path.

For a fuller maintenance routine, see drawstring garbage bag machine daily maintenance and troubleshooting.

When Hardware, Not Adjustment, Is the Answer

Some tension problems cannot be tuned away:

● Speed above 70 m/min with a friction-only tape control — friction varies with temperature and wear, and no amount of adjustment makes it repeat at speed. A servo-driven tape axis is the fix.

● Frequent bag width changes — if the tape path has to be re-threaded and re-tensioned for every width, the cost is in changeover time. A path with fixed guides and a movable stop pays for itself quickly.

● Tape grades from multiple suppliers — different friction coefficients mean different settings for each. A load cell system that holds actual tension removes the need to re-tune per supplier.

● Consistent complaints from one customer only — check whether their filling or packing process pulls the bag differently. Occasionally the machine is right and the complaint is about a use case the bag was not designed for.

The CW-1000PG perforated roll draw tape machine is a useful reference point for what a tape path looks like when it is designed for servo control from the start: separate drive, dedicated dancer and a guide set that does not need re-threading for every width.

Chasing a tape defect that returns every few rolls?
Send a photo of the defect and the bag size. We will tell you which zone of the tape path is responsible, and whether the fix is a setting, a wear part, or a change in the tape specification.

Send a Tape Defect for Diagnosis

Frequently Asked Questions

What causes wrinkles along the hem on a draw tape bag?

Almost always excess tape tension or a tape entering faster than the film. Check the drive ratio between tape and film first, then reduce tape tension in small steps. A puckered hem that appears only as the tape roll empties points to a control that is not compensating for diameter.

How tight should the draw tape be inside the hem?

Tight enough to lie flat without puckering, loose enough that the tape slides when pulled. Test at full, half and near-empty tape roll diameter; a setting that works at one diameter and not the others is a control problem rather than a setpoint problem.

Why does the drawstring pull out of the hem?

The hem seal did not capture the tape. Common causes are tape sitting too deep, sealing temperature too low, or a hem fold that was not flat before sealing. Check the fold first, because no temperature increase will seal a hem that is folded over itself.

Can I run different tape thicknesses on the same machine?

Yes, within the range the tape path was designed for. Each thickness needs its own tension setting and, in some cases, a different hem seal temperature. Record the settings per tape grade so a change does not become a re-tuning exercise.

How often should tape path rollers be checked?

Weekly by hand: spin each roller and confirm it coasts. Any roller that drags adds tension that varies with load, which is exactly the kind of fault that produces intermittent defects nobody can reproduce.

Does machine speed affect tape tension?

Yes. Higher speed shortens the response time available to any tension control, so a dancer that holds tension at 30 m/min may oscillate at 60 m/min. If defects appear only at high speed, the control hardware is the constraint, not the setting.

What tape width should a 900 mm bag use?

Width is usually matched to the hem depth rather than the bag width, and 25 to 35 mm is common for consumer rolls. Confirm the hem fold depth on your machine before ordering tape, because a tape wider than the hem cannot be sealed in without puckering.

Related Resources

● Drawstring Garbage Bag Machine: Daily Maintenance and Troubleshooting — the maintenance side in detail.

● How a Garbage Bag Roll Machine Supports Small, Medium and Large Roll Formats — winding side of the same line.

● How Garbage Bag Making Machines Work — the full process from film to roll.

Coming next: Tape Grade Selection for Draw Tape Bags: Width, Thickness and Friction, and Why Drawstring Bags Fail at the Hem Fold.

GET A QUOTE NOW